From Explorator 5.8
The Telegraph and Wshington TImes have versions of the Rievaulx Abbey blast
furnace story.
http://portal.telegraph.co.uk/news/main.jhtml?xml=%2Fnews%2F2002%2F06%2F21%2Fnhenry21.xml
http://www.washtimes.com/world/20020622-67190988.htm
The story has been revived as Bradford and English Heritage were trying do some
experimental reconstructions on Friday. Gerry - was it successful?
Chris Salter
---------------------------------------------
JXA-8800 Superprobe, Electron Microscopy Facility
Department of Materials,
Begbroke Business and Science Park,
Sandy Lane,
Yarnton,
Oxford OX5 1PF,
Tel. Office 01865 283722
Probe 01865 283741
Fax. 01865 848790
Mobile. 0777 6031608
E-mail [log in to unmask]
|