Omid, I have a copy but it is rather large. Contact me off list and I will send it to you. Aaron On Mon, Feb 11, 2019 at 9:17 AM Salzmann, Eveline < [log in to unmask]> wrote: > Dear Omid, > > I think, you mean this book: > > Hauptmann, H. and Pernicka, E., eds., 2004. *Die Metallindustrie > Mesopotamiens von den Anfängen bis zum 2. Jahrtausend v. Chr. *Rahden > /Westf. > > > > Although there is no article in it by Begemann & Schmitt-Strecker, but > from Müller-Karpe, Helwing & Müller, Lutz & Pernicka. Including a lot of > XRF and INAA analyses from Mespotamian artefacts. > > > > If you mean the article, where Begemann & Schmitt-Strecker analysed also > lead isotopes of Mesopotamian copper based artefacts, then it would be from > 2009: > > > > Begemann, F. and Schmitt-Strecker, S., 2009. Über das Frühe Kupfer > Mesopotamiens. *Iranica Antiqua, (*44), pp. 1–45. > > > > Best wishes, > > Eveline > > > > > > *Von:* Arch-Metals Group [mailto:[log in to unmask]] *Im Auftrag > von *Omid Oudbashi > *Gesendet:* Montag, 11. Februar 2019 14:12 > *An:* [log in to unmask] > *Betreff:* Request for a Paper > > > > Dear Colleagues, > > > > I am searching to find the following published work about LIA analysis of > copper alloys from Mesopotamia. It has been cited in some published works > with different dates (2004, 2006, 2008), but I couldn't find the > paper/chapter. > > I would be so appreciated of you if send me a copy of this paper. > > > > Begemann, F. and S. Schmitt-Strecker 2006 “Materialanalysen, > Untersuchungen zur Herkunft der Rohstoffe, in Die Metallindustrie > Mesopotamiens von den Anfängen bis zum 2. Jahrtausend v. Chr.”, H. > Hauptmann and E. Pernicka (eds.) Orient-Archäologie. Rahden/Westfahlen. > > > > Kind Regards > > > > Omid > > > > > > --------------------------------------------------------------------- > > *Omid Oudbashi* > > PhD in Conservation of Cultural and Historical Properties > > > *Assistant Professor and Head of the Central Laboratory, **Department of > Conservation of Cultural and Historical Properties and Archaeometry*, > > Faculty of Conservation, Art University of Isfahan > > Address: P.O.Box: 1744, Isfahan, Iran > Email: [log in to unmask]; [log in to unmask] > Website: www.aui.ac.ir > > > ------------------------------ > > To unsubscribe from the ARCH-METALS list, click the following link: > https://www.jiscmail.ac.uk/cgi-bin/webadmin?SUBED1=ARCH-METALS&A=1 > ------------------------------ > > *Eveline Salzmann *Archäometallurgie > *Telefon:* > *Fax:* > *E-Mail:* [log in to unmask] > > Deutsches Bergbau-Museum Bochum > Herner Straße 45 > 44787 Bochum > http://www.bergbaumuseum.de > http://www.facebook.de/bergbaumuseum > ------------------------------ > > > > > > > > > *Eine Einrichtung der DMT-Gesellschaft für Lehre und Bildung mbH Sitz der > Gesellschaft: Bochum Registergericht: Amtsgericht Bochum Handelsregister: B > 4052 Geschäftsführung: Prof. Dr. Jürgen Kretschmann (Vorsitzender) Adolf > Siethoff * > > ------------------------------ > > To unsubscribe from the ARCH-METALS list, click the following link: > https://www.jiscmail.ac.uk/cgi-bin/webadmin?SUBED1=ARCH-METALS&A=1 > -- Aaron Shugar [log in to unmask] [log in to unmask] http://flip.it/fCmAh ######################################################################## To unsubscribe from the ARCH-METALS list, click the following link: https://www.jiscmail.ac.uk/cgi-bin/webadmin?SUBED1=ARCH-METALS&A=1