Message text written by INTERNET:[log in to unmask]
><
William
I think that the analysis you have given us for the lowest slag melting
temperature shows why bloomeries can easily deal with titaniferous ore
while charcoal blast furnaces might struggle to make iron. Your lowest
melting point slag has 15% FeO. This is around ten times the usual level
found in blast furnace slag.
Peter
%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
|