Hello What is the theoretical composition of iron slag and should such slag react with 10% hydrochloric acid (i.e. does it contain CaCo3)? Thanks jeremy %%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%