Forwarded from Historical Archaeology.
Please reply Directly to Ian Burrow as he is not on arch-metals.
-------- Original Message --------
Subject: Slag Analysis
Date: Fri, 5 Jul 2002 11:10:01 -0400
From: Ian Burrow <[log in to unmask]>
Reply-To: HISTORICAL ARCHAEOLOGY <[log in to unmask]>
Organization: Hunter Research, Inc.
To: [log in to unmask]
Can anyone direct me to someone who is currently doing analysis of slags
from historic archaeological sites? We are preparing to work at a 19th
century blacksmith shop site and would like to follow the methodology
used by Light and Unglik in the Fort St Joseph (Ontario) study, but we
need a metallurgist to do the x-ray fluorescence and associated
analyses. Thanks in advance Ian BurrowHunter Research, Inc.
|