Mark
19th century wrought iron and medieval wrought iron are quite different.
Most 19th century wrought iron was a fairly cheap mass produced product.
Peter Nothover has examined some railway track and was apalled at how poor
the quality was. Similar comments were made about the iron used for the
Titanic. The best was reserved for jobs such as anchor and lifting chains.
The iron used for these had to be capable of being tied hot into a loose
overhand knot and pulled up tight cold without any cracking.
Medieval wrought iron was an expensive craft product. It was probably a
matter of careful attention to the production variables such as the ore
used, the charcoal, and the temperature at which the bloom was made and
forged. The final test was probably to try a bit. Like all Medieval crafts
almost nothing was written down perhaps because the craftmen could not read
or write.
I expect there were horses for courses. The wire drawers would know or
employ a smith who usually produced the right quality. Drawn wire is, of
course, quite different from the sizing operation you have described. I do
not see how you would tell whether the base material was slit from a plate
by examining the finished wire.
The modern steel industry (and most other industry) works in a similar
manner, though controlling the process is more accurate. Testing (which is
really only trying a bit) is to find out whether you got it right. If you
didn't all the processing is wasted. Only at a very few points can things
possibly be put right. As in Medieval times you may be able to sell the
lower grade material. In the 1960s if it was sheet steel and flattish
someone would buy it but not now.
Peter Hutchison
|