James Bothers wrote
>What are the liquidus temperatures of hematite and magnetite<
James
>From my chemistry book (Partington)
Ferric oxide loses some oxygen above 1200deg C and melts at 1563 deg C.
Ferrosoferric oxide melts at 1540 deg C
This is. of course, the pure stuff not the ore.
Peter Hutchison
%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
|