There is very little discussion of foundry operations in the iron industry
literature. How does foundry slag differ from bloomery and finery slag? I am
interested in both visually (macro and micro) and chemically.
JH Brothers IV
%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
|