> The hot-coated pieces I have examined are all rein-rings from bronze
> plated iron horse bits. The microstructures show clearly that the iron
> has been in contact with molten bronze.
Dear Peter,
my question is : how the microstructures created by dipping and by
"soldering" will be different in order to distinguish clearly between
different manupulations using approximatively the same material under
comparable temperature conditions.
Ingo
%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
|