I have C71X07:
Cu |
Sn |
Pb |
Zn |
Ni |
Fe |
Mn |
As |
Sb |
|
C71X07 |
83.66 |
6.1 |
4 |
5.2 |
0.51 |
0.08 |
0.01 |
0.2 |
0.22 |
I have other BNF standards, but not any on your list.
Matthew Ponting BA PhD FSA
RACOM – ERC funded research project
Senior Lecturer in Archaeological Materials
Archaeology, Classics and Egyptology
The University of Liverpool
12/14 Abercromby Square
Liverpool
L69 1WZ
Tel: 0151-794-4393
From: Arch-Metals Group <[log in to unmask]>
On Behalf Of Benzonelli, Agnese
Sent: 28 October 2021 11:02
To: [log in to unmask]
Subject: BNF standard composition
Dear all,
Does anyone have the composition/certificates of these BNF standards?
Cupro-Nickel: C62X07
Cupro-Nickel: CN1C
Cupro-Nickel: CN5B
Gun metal: C71X07
Gun metal: GM3A
Nickel-silver: C65X17
Thank you and best wishes, Agnese
--
Dr. Agnese Benzonelli
Technician in archaeomaterials preparation and analysis
UCL Institute of Archaeology
31-34 Gordon Square
London, WC1H 0PY
To unsubscribe from the ARCH-METALS list, click the following link:
https://www.jiscmail.ac.uk/cgi-bin/WA-JISC.exe?SUBED1=ARCH-METALS&A=1