JG.McDONNELL wrote:
>
> hammerscale is (normally) highly magnetic, comprising magnetite, possible
> some small percentage of metallic iron, the oxides fused by a
> 'glasy/fayalitic' phase.
If you want to have a look at (platy) hammerscale, here it is
(recent material: Heinz Denig, Kaiserslautern/Trippstadt, Germany):
http://www.uni-mainz.de/FB/Geo/Geologie/archaeo/Hammerschlag.gif
Ingo Keesmann