Ploquin Alain wrote:
> >I'm working on an MA in Historical Archaeology. My topic is the 17/18C
> >furnaces
> >of Virginia. Is there any data on the viscosity of blast furnace slags? What
> >are typical poise values for Ca-Si slags?
> >
> >JH Brothers IV
> >Wm. & Mary
> ********************
> Viscosity is fonction of composition, temperature and polymerisation of the
> liquid (melt). In the "Schlaken Atlas" edited by the VDE (a german
> association for metallurgists), many diagramms are available.
> A.Ploquin
>
> Alain Ploquin
> Centre de Recherches Petrographiques et Geochimiques (UPR A9046)
> Centre National de la Recherche Scientifique
> B.P.20
> F-54501 Vandoeuvre-les-Nancy cedex
> France
> tel: 33/(O)383594245 fax: 33/(0)383511798
To be more specific. Is there data from 17/18th century blast furnaces? How much
of a data base is there? I have access to the Schlackenatlas.
Thanks
JH Brothers IV
%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
|