Peter Hutchison wrote:
> Jamie
>
> We used to dry our steel samples with industrial alcohol and store them in
> a dessicator with silica gel as a dessicant.
>
> Peter (ex steelworks metallurgist)
I suppose I could work at it with some kind of polishing rouge then dry it off
with alcohol. Might work.
Thanks
Jamie
%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
|