Olfert Voss, try address National Museum, Frederiksholms Kanal 12, DK-1220 Copenhagen K, Denmark.
He has some good photographs of large complete chimney furnace iron slags.
-----Original Message-----
From: [log in to unmask]
[mailto:[log in to unmask]]On Behalf Of James H Brothers
IV
Sent: 24 September 1999 14:38
To: arch-metals
Subject: Slag and Blooms
I would like to include pictures of blooms and slags in a paper I'm writing.
Although I have slag samples from a variety of blast furnaces. I have nothing
from bloomeries. There are very few excavated bloomeries in the US. I am
looking for macro not micro, suitable for use by field archaeologists. Would
anyone be willing to share illustrations of blooms and slags? If so I can read
just about any electronic format or can scan photographs. Good pictures of
furnace slags would also be useful.
Thank You
JH Brothers IV
%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
|