Trevor Umber is the name given to the manganese-rich equivalent of ochre Best wishes Tim -- Dr Tim Young MA PhD FGS FSA Email: [log in to unmask] Web: www.geoarch.co.uk Phone: 07802 413704 Fax: 08700 547366