Hi David,
Is it possible to etch electrum and get any useful information? Would it almost always be solid solution... would that depend on the ratio of gold to silver?
Do you know of any articles/results or photomicrographs or anyone who specializes in studying electrum? I'm doing some research on some Lydian electrum coins in the Harvard collection.
Thanks,