JiscMail Logo
Email discussion lists for the UK Education and Research communities

Help for ARCH-METALS Archives


ARCH-METALS Archives

ARCH-METALS Archives


ARCH-METALS@JISCMAIL.AC.UK


View:

Message:

[

First

|

Previous

|

Next

|

Last

]

By Topic:

[

First

|

Previous

|

Next

|

Last

]

By Author:

[

First

|

Previous

|

Next

|

Last

]

Font:

Proportional Font

LISTSERV Archives

LISTSERV Archives

ARCH-METALS Home

ARCH-METALS Home

ARCH-METALS  November 2009

ARCH-METALS November 2009

Options

Subscribe or Unsubscribe

Subscribe or Unsubscribe

Log In

Log In

Get Password

Get Password

Subject:

Ang: Re: Ang: Re: slag rods/tubes on archaeological sites

From:

Anders Söderberg <[log in to unmask]>

Reply-To:

Anders Söderberg <[log in to unmask]>

Date:

Thu, 19 Nov 2009 11:23:44 +0100

Content-Type:

text/plain

Parts/Attachments:

Parts/Attachments

text/plain (211 lines)

Hello again Sébastien, and everybody else,

I do recognize the object at your picture. There's at least 
one similar object from Helgö, see http://hem.passagen.se/anders.sberg/9890.jpg

This is an end-piece from a ceramic package from some 
metallurgical process where the iron object to be treated was 
wrapped in a protecting clay package before treatment. There 
are probably several processes where clay was used in this way, 
and I know two that so far have been identified - case 
hardening and brazing (usually of padlocks and bells) - and 
probably there may be a package-welding process around as well, 
but the ceramic remains from such a process haven't yet been 
identified.

The "Propfen" could represent end pieces from treating tubular 
iron objects, as suggested at left in the picture 9890.jpg - 
perhaps from soldering together/brazing small bells.

There are a few more examples from Bosau: check "Gebers, W. 
1981. Bosau, Untersuchung einer Siedlungskammer in 
Ostholstein. V:1, Der slawische Burgwall auf dem 
Bischofswarder. Teil 1: Katalog. Sackau, H. (red) Neumünster.", 
tafel 22, page 120.

Picture 4, 5 and 6 show similar end pieces. Moreover, picture 
1, 2 and 3 show exellent fragments from brazing padlocks, with 
visible imressions of the locks, and pictures 8-16 show 
different examples of tubular packages, probably deriving from 
case hardening.

Anders


>----Ursprungligt meddelande----
>Från: [log in to unmask]
>Datum: 18-11-2009 21:18
>Till: <[log in to unmask]>
>Ärende: Re: Ang: Re: slag rods/tubes on archaeological sites
>
>An image is avaible here: http://www.zoyd.info/public/bouchons.jpg.

>These two examples are from a large gallo-roman rural smithy 
in 
>Etagnières/Switzerland. As far as I can remember, some other 
pictures 
>were published in the monographs of Haithabu (viking/Germany) 
and 
>Dietikon (roman/Switzerland), but I don't have them at hand 
right now; 
>however, besides of the section, all of these items look quite 
similar. 
>I might put some other photographs online, if useful.
>Cheers, Sébastien
>
>Anders Söderberg a écrit :
>> It would be most interesting to see a few pictures of those 
>> "Propfen". Are there any available somewhere?
>>
>> Anders
>>
>>
>>   
>>> ----Ursprungligt meddelande----
>>> Från: [log in to unmask]
>>> Datum: 18-11-2009 16:10
>>> Till: <[log in to unmask]>
>>> Ärende: Re: slag rods/tubes on archaeological sites
>>>
>>> Dear all,
>>>
>>> I guess we may be talking of different things, but I 
thought 
>>>     
>> I might use
>>   
>>> this occasion to query about some slightly similar pieces 
for 
>>>     
>> which I don't
>>   
>>> find any satisfying explanation. We repeatedly found some 
clay 
>>>     
>> rods a few
>>   
>>> centimetres long in slag assemblages of gallo-roman 
smithies 
>>>     
>> in Switzerland
>>   
>>> (I know of at least 6 individuals from three sites in 
>>>     
>> Switzerland). The
>>   
>>> surfaces are blackish and slagged on a very shallow 
surface. 
>>>     
>> They have an
>>   
>>> oval or rectangular section of perhaps three or four 
>>>     
>> centimeters; one
>>   
>>> extremity generally shows a slight bulge. The pieces are 
>>>     
>> altered on all
>>   
>>> surfaces of this extremity, which was obviously exposed to 
a 
>>>     
>> certain heat,
>>   
>>> although the alteration is restricted to the surface. One 
of 
>>>     
>> these pieces
>>   
>>> was analysed some time ago by Marianne Senn; the surface 
was 
>>>     
>> strongly
>>   
>>> enriched in iron, and the clay seemed to be similar to 
that 
>>>     
>> used for crucibles.
>>   
>>> Similar pieces have been found in quite large numbers in 
the 
>>>     
>> Viking site of
>>   
>>> Haithabu, and two or three others are known from two French 
La 
>>>     
>> Tène sites. I
>>   
>>> guess there might be many others, but they are quite 
difficult 
>>>     
>> to identify
>>   
>>> in large slag assemblages; besides of the particular 
>>>     
>> morphology, the
>>   
>>> material looks just like the usual sandy-clayey slags; 
like 
>>>     
>> these, they are
>>   
>>> probably quite friable.
>>>
>>> The pieces I know of are always clearly associated to 
smithies 
>>>     
>> in sites
>>   
>>> devoid of smelting activities. In german, they have been 
>>>     
>> called "Propfen" or
>>   
>>> "Zapfen". Obviously, they were used to block some 
rectangular 
>>>     
>> or ovoid
>>   
>>> opening (an air inlet?) on one side of the hearth exposed 
to 
>>>     
>> the fire; but
>>   
>>> why would there be a need to block an air inlet in a 
smithing 
>>>     
>> hearth (and
>>   
>>> what is more, from the inside)? Although they seem to be 
very 
>>>     
>> rare, I find
>>   
>>> it astonishing to find such pieces all over the time from 
Iron 
>>>     
>> Age to
>>   
>>> medieval times. I just can't figure out to what particular 
>>>     
>> practice they
>>   
>>> could be associated; I wonder if somebody could come up 
with 
>>>     
>> some
>>   
>>> explanation for these objects?
>>>
>>>     
>
>-- 
>Sébastien Perret
>Mineralogy and Petrography, Department of Geosciences
>University of Fribourg, Chemin du Musée 6, CH-1700 Fribourg, 
Switzerland
>phone: +41 (0)26 300 89 40
>mail: [log in to unmask] <mailto:[log in to unmask]
ch> 
><http://www.unifr.ch/geoscience/mineralogy/archmet>>

Top of Message | Previous Page | Permalink

JiscMail Tools


RSS Feeds and Sharing


Advanced Options


Archives

May 2024
April 2024
March 2024
February 2024
January 2024
December 2023
November 2023
October 2023
September 2023
August 2023
July 2023
June 2023
May 2023
April 2023
March 2023
February 2023
January 2023
December 2022
November 2022
October 2022
September 2022
August 2022
July 2022
June 2022
May 2022
April 2022
March 2022
February 2022
January 2022
December 2021
November 2021
October 2021
September 2021
August 2021
July 2021
June 2021
May 2021
April 2021
March 2021
February 2021
January 2021
December 2020
November 2020
October 2020
September 2020
August 2020
July 2020
June 2020
May 2020
April 2020
March 2020
February 2020
January 2020
December 2019
November 2019
October 2019
September 2019
August 2019
July 2019
June 2019
May 2019
April 2019
March 2019
February 2019
January 2019
December 2018
November 2018
October 2018
September 2018
August 2018
July 2018
June 2018
May 2018
April 2018
March 2018
February 2018
January 2018
December 2017
November 2017
October 2017
September 2017
August 2017
July 2017
June 2017
May 2017
April 2017
March 2017
February 2017
January 2017
December 2016
November 2016
October 2016
September 2016
August 2016
July 2016
June 2016
May 2016
April 2016
March 2016
February 2016
January 2016
December 2015
November 2015
October 2015
September 2015
August 2015
July 2015
June 2015
May 2015
April 2015
March 2015
February 2015
January 2015
December 2014
November 2014
October 2014
September 2014
August 2014
July 2014
June 2014
May 2014
April 2014
March 2014
February 2014
January 2014
December 2013
November 2013
October 2013
September 2013
August 2013
July 2013
June 2013
May 2013
April 2013
March 2013
February 2013
January 2013
December 2012
November 2012
October 2012
September 2012
August 2012
July 2012
June 2012
May 2012
April 2012
March 2012
February 2012
January 2012
December 2011
November 2011
October 2011
September 2011
August 2011
July 2011
June 2011
May 2011
April 2011
March 2011
February 2011
January 2011
December 2010
November 2010
October 2010
September 2010
August 2010
July 2010
June 2010
May 2010
April 2010
March 2010
February 2010
January 2010
December 2009
November 2009
October 2009
September 2009
August 2009
July 2009
June 2009
May 2009
April 2009
March 2009
February 2009
January 2009
December 2008
November 2008
October 2008
September 2008
August 2008
July 2008
June 2008
May 2008
April 2008
March 2008
February 2008
January 2008
December 2007
November 2007
October 2007
September 2007
August 2007
July 2007
June 2007
May 2007
April 2007
March 2007
February 2007
January 2007
2006
2005
2004
2003
2002
2001
2000
1999
1998


JiscMail is a Jisc service.

View our service policies at https://www.jiscmail.ac.uk/policyandsecurity/ and Jisc's privacy policy at https://www.jisc.ac.uk/website/privacy-notice

For help and support help@jisc.ac.uk

Secured by F-Secure Anti-Virus CataList Email List Search Powered by the LISTSERV Email List Manager