There is another source for x-ray emission lines. It is
http://physics.nist.gov/PhysRefData
Then look for x-ray transition energies
The listing is either in Angstroms or in energies and may be sorted by
element or range.
The biggest problem using these tables is that second and higher order
emission lines are not listed. I usually use a hand calculator to find
these.
Sincerely,
Ed Sharp
===============================================
On Mon, 7 Jul 2008, Bastian Asmus wrote:
> Hello everyone,
>
> this is just to let you know that there is a new online service for
> checking x-ray emission line overlaps. We thought this might be
> especially useful if you are not so sure where the sometimes
> problematic line overlaps are.
> You can specify the element as well as the range around the
> characteristic x-rays. The script checks for the Ka1, Ka2, Kb1, Kb2,
> La1, La2, Lb1, Lb2, Lg1 and Ma1 lines.
> http://www.ucl.ac.uk/archmat/tools/emission.php
>
> Please feel free to contact me if there are any suggestions or mistakes.
>
> best,
> Bastian
>
>
>
> ---
> Bastian Asmus
> Marie Curie EST Research Fellow
> Archaeometallurgy
> UCL, Insitute of Archaeology
> University College London
> 31-34 Gordon Square
> London WC1H 0PY
>
>
>
>
--
[log in to unmask]
|