Re: medieval bronze bells in Western Europe
From:
david bourgarit <[log in to unmask]>
Reply-To:
Arch-Metals Group <[log in to unmask]>
Date:
Tue, 1 Jul 2008 11:43:15 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (5 lines)
Justine, in waiting for your papers, may I just ask you what do you mean by low lead level ? In the french bells from 12th to 15th, lead is around 3w% ...