I found a piece of metal on the surface of Huluga, an archaeological
site in Cagayan de Oro, Philippines:
http://elson.elizaga.net/huluga-metal2.html
Dr. Erlinda M. Burton, an archaeologist here, told me it might be part
of a sword. A Copper 8 Maravedis coin was also found in this site.
See the coin and other artifacts:
http://heritage.elizaga.net/huluga/artifacts/index.html
I would be glad if anyone could help me identify the piece. It doesn't
look like anything native that I've seen.