HAPPY NEW YEAR!liyanxiang
在您的来信中曾经提到:
>From: W H <[log in to unmask]>
>Reply-To: Arch-Metals Group <[log in to unmask]>
>To: [log in to unmask]
>Subject: Re: chinese bronze composition
>Date:Thu, 7 Feb 2008 12:48:16 +0800
>
>I am sorry that I am not in China now so can not check out these Chinese
>book.
>But you can refer to the documents published by British Museum and Freer
>Gallery of Art, maybe there are some information on this topic.
>the Zn content is very high, I do not think it is the Han dynasty's objects,
>because ancient Chinese craftsmen mastered zinc smelting technology in the
>Ming dynasty to acquire this high Zn content according to the combinational
>study of Paul. Craddock and Weirong Zhou
>
>good luck
>
>2008/2/7, Bart (comcast) <[log in to unmask]>:
>>
>> Are there any references in English or would someone be willing to check
>> out
>> these Chinese sources for me?
>>
>> I am trying to match the composition of two bowls that have been dated, on
>> stylistic criteria, as being post-Han to pre-Yuan era. Below are the
>> compositions of the bowls measured by XRF.
>>
>>
>> ELEMENT copper Zinc lead tin iron bismuth nickel chromium
>> vanadium cobalt
>> First Bowl 59.52 32.64 3.40 1.92 1.36 0.52
>> 0.24
>> ---- 0.02 ----
>> Second Bowl 61.39 30.06 4.07 1.78 1.29 0.56
>> 0.19
>> 0.13 0.02 0.07
>>
>> Thank you for any help.
>>
>> Bart
>> [log in to unmask]
>>
>> -----Original Message-----
>> From: Arch-Metals Group [mailto:[log in to unmask]] On Behalf Of
>> Wei
>> Huang
>> Sent: Thursday, January 31, 2008 9:13 PM
>> To: [log in to unmask]
>> Subject: Re: chinese bronze composition
>>
>>
>> hi,
>> there are two Chinese Books on the composition of ancient bronze which
>> collect almost the all bronze analysis data in China, you can find the
>> Chinese bronze composition that you need really.
>> 1. Zhong guo shang gu jin shu ji shu (Metalworking technology of Ancient
>> Chinese), by shu rong yu, hua jue ming etc. Shan dong ke xue ji shu chu
>> ban she(press of science and technology of shan dong)
>>
>> 2. The Chinese history of science and technology-metallurgy, published in
>> 06 or 07, science press in China
>>
>
>
>
>--
>Huang Wei
>
>Doctoral Candidate
>School of Archaeology and Museology
>Peking University
>Beijing 100871 China
>
>UCLA/Getty Conservation Program
>Cotsen Institute of Archaeology
>University of California Los Angeles CA 90025 USA
>
>
>Powered by MessageSoft SMG
>SPAM, virus-free and secure email