Dear Trevor,
We are in a position to help you with the analysis - with non-ferrous
materials I tend to prepare the samples and Chris Salter does the
analysis. Depending on the complexity of the sample the analysis we
provide would cost in the range £30-£50 per sample + VAT for up to 17
elements. That will provide the basic analysis plus metallographic
image. I hope this helps.
Yours,
Peter
--
Dr Peter Northover,
Materials Science-Based Archaeology Group,
Department of Materials, University of Oxford
Tel +44 (0)1865 283721; Fax +44 (0)1865 841943 Mobile +44 (0)7785 501745
e-mail [log in to unmask]
|