Re: Agricultural slag
From:
Peter Hutchison <[log in to unmask]>
Reply-To:
Date:
Thu, 11 Mar 2004 15:01:31 -0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (5 lines)
BOS and basic open hearth slag "perish" due to the lime content and are not suitable for aggregate or hardcore. Peter