JiscMail Logo
Email discussion lists for the UK Education and Research communities

Help for ARCH-METALS Archives


ARCH-METALS Archives

ARCH-METALS Archives


ARCH-METALS@JISCMAIL.AC.UK


View:

Message:

[

First

|

Previous

|

Next

|

Last

]

By Topic:

[

First

|

Previous

|

Next

|

Last

]

By Author:

[

First

|

Previous

|

Next

|

Last

]

Font:

Proportional Font

LISTSERV Archives

LISTSERV Archives

ARCH-METALS Home

ARCH-METALS Home

ARCH-METALS  2002

ARCH-METALS 2002

Options

Subscribe or Unsubscribe

Subscribe or Unsubscribe

Log In

Log In

Get Password

Get Password

Subject:

Re: Steelmaking at Wortley Top Forge

From:

Peter King <[log in to unmask]>

Reply-To:

Arch-Metals Group <[log in to unmask]>

Date:

Wed, 17 Jul 2002 15:20:51 +0100

Content-Type:

text/plain

Parts/Attachments:

Parts/Attachments

text/plain (210 lines)

One problem is that the term 'German steel' is used for two different
commodities.  One was Styrian steel,  which was imported in relatively small
quantities, usually as 'long German steel'.  The other was made in England
from blister steel.  It seems to me (but I do not have clear evidence) that
for a few purposes where an extremely hard material was needed Styrian steel
was used.  Such uses include drawplates for wiremills and cutters for
slitting mills.  However the use of imported steel is the exception in this
period.  The vast majority of the steel used in England in the 18th century
was blister steel and products derived from it, such as crucible steel and
shear steel.  Almost all of this was made from a special kind of Swedish
iron (oregrounds) made from ore from the Dannemora mine,  with a  smaller
amount of less good quality steel made from Russian 'Old Sable iron', though
the evidence for the use of Sable iron comes only from the Crowley works
near Newcastle.

For most of the Cockshutt period at Wortley,  charcoal iron (such as that
made at Bank, Barnby and Bretton Furnaces) was not used in foundries,  but
certain parts for hammers etc. were cast direct from the furnace.  When worn
out or broken these were probably worked up into bar iron as if they were
pig iron.  However the normal cast iron goods were by this time mostly made
with coke pig iron.  In the 1720s pots and kettles made at Coalbrookdale
were being sold to John (I think) Ivie at Gainsborough,  probably a
wharfinger there,  who was no doubt acting as a wholesaler for their
distribution into Lincolnshire and Yorkshire.  There was also a foundry at
Newcastle,  associated with a coke furnace (Little Clifton) near Whitehaven
and later Whitehill near Chester le Street.  The earliest Sheffield foundry
I have traced goes back to about 1760,  and this is not long after the
Walkers built their coke furnace near Rotherham.  I would therefore suspect
that the foundry at Wortley would not have been needed until its owners no
longer had their own charcoal furnace and therefore wanted a means of
producing specialised casting for their own use.  Something similar happened
at Cookley in north Worcestershire.

I am copying this to another list,  which specialises in the history and
archaeology of metallurgy.


Peter King,
49, Stourbridge Road,
Hagley,
Stourbridge
West Midlands
DY9 0QS

telephone 01562-720368
----- Original Message -----
From: Dr. Chris Morley <[log in to unmask]>
To: <[log in to unmask]>
Sent: 17 July 2002 09:33
Subject: Steelmaking at Wortley Top Forge


Paul Bedford queried the possibility of steel making at Wortley. I put
forward my findings upon the subject, and confirm that I think that the
remains are of a reverboratory furnace, possibly for the purpose of melting
pig iron. But, there again, it may have been one of the several puddling
furnaces erected by James Cockshutt following his return from South Wales -
possibly his first experimental furnace?

At the Top Forge site it is possible that a small Foundry had been
established, possibly for cast iron products and spare parts such as gear
wheels for the Iron Works.

In 1977, excavations at the south-west end of the Top Forge site revealed
the
foundations of what has been variously interpreted as being a steel
cementation furnace, or an iron-melting reverberatory  furnace. If the
remains are of the former then this would bear out the claim of Schubert
that
John Cockshutt, either I or II, which one  we are not quite sure, produced
shear steel at Wortley in the middle of the 18th. century. The Cockshutt’s
certainly used ‘German’ steel  - otherwise known as Shear Steel - for the
manufacture of drawing plates for their wire works on account of its
hardness
for drawing Steel wire. The remains, however, clearly show an end flue
consistent with the arrangement of a reverberatory furnace and not a
cementation furnace, and they are at the outer end of a building which has
traditionally been known as ‘the Foundry’. Cockshutt could have obtained
sufficient supplies of blister steel for his needs from the Grenoside
cementation furnace that the Walkers had built during the period
1749-1750. His supply from Nether Bank and Bretton Furnaces would also
ensure
a ready amount of pig iron to remelt for cast iron production and other cast
iron machinery products to be made ‘on site’. His Millwrights, David
Burkinshaw and, later, Joel Jagger, were skilled moulding pattern makers,
and
indeed a ‘pattern maker’ was employed at the Top Forge site up until it
closed down in 1908.
    However, the late Dr. Ken Barraclough, Secretary, and later President,
of
the Sheffield Trades Historical Society, wrote the following to members of
the Council of Management of the South Yorkshire Trades Historical Trust in
November 1976 upon the subject:

    'The excavations at the end of the ‘Foundry’ building at Wortley Top
Forge have revealed a structure plan which, merely  judging by the fire
attack on the walls adjacent, must have been a furnace. This furnace itself
seems to be surrounded by walls which are not keyed into the adjoining
building, which itself has been variously dated but in any case would seem
not to be earlier than the Forge extensions themselves in 1713, and which
may
well be later.
    The inner furnace wall, as it may now be called since there would appear
to be an outer retaining wall not yet excavated, shows a chute entry on the
end nearest the road, this chute being blocked off at its end and at this
stage by a stone built infilling in the wall below. Of the two long walls,
the one nearer the river is intact but fire attacked; the opposite wall,
however, has a large patch midway along it's length filled in with brick;
this brick seems to be a similar type to that in the arch in the Foundry
building end and could possibly be of late 18th. century date from it's
appearance.  The floor surrounded by these walls is generally of brick,
which
appears to be  of a similar type to the above. There are, however, two rows
of three stone blocks set symmetrically along the length; five of these
carry
two square holes each whilst the six has only one.
    Examination of the debris in the lower layers and in the channels
between
the stone blocks has provided charcoal, coal, a red powder high in iron
oxide, fire-reddened pieces of sandstone, and a light slag, which seems to
be
partially fused brick.
    It has always been inferred that, in the period when the forge at
Wortley
was in the hands of the Cockshutts, considerable experimentation was carried
out there and there are certainly references to steelmaking carried out by
them (the Cockshutts), although it is not certain that this was at Wortley,
although Schubert implies that this was so. Certainly the remains we have
recently uncovered rather encourage the idea that we may well here have the
evidence of such operations, particularly as the plan so revealed is
strikingly similar to those on the attached illustration, which comes from
‘Siderotechnie’, a comprehensive treatise in French on iron and steel
manufacture, published in Paris in 1812. This shows a number of cementation
furnaces, among others those at Swalwell (Figure A, B, C, and D.) and a
single chest furnace operating in Sheffield in 1767 (K. and I.). Those of
paramount interest in this context are the two examples G/H and L/M, both of
which show a chute at the end and built up piers of masonry. Such a furnace
with a modified chimney structure, bringing the exit to the end of the
structure so as to give the chimney ghost outline on the Foundry wall, would
account for most of the features seen at Wortley.'

    Barraclough wrote an article published in the Journal of The Historical
Metallurgy Society, vol. 11, No. 2, 1977, p. 88: Wortley Top Forge, the
possibility of early steel production, in which he clearly states his
opinion
of the furnace remains. Illustrations of a possible design of the furnace
were included.

    The reference in the above to Schubert is from page 329 (History of the
British Iron and Steel Industry) where he, Schubert, writes:

     'In the eighteenth century the principal production of shear steel was
near to Newcastle-upon-Tyne, at Ambrose Crowley’s steelworks. Another centre
was at Wortley in Yorkshire, where John Cockshutt took up the manufacture in
the middle of the century, but the steel he made was not of such a high
repute as Crowley’s. English shear steel, in particular Crowley’s, proved to
be superior to contemporary German steel produced in Styria and the Tyrol
and
up to then imported in large quantities into England. English cutlers who
had
formerly employed it in the manufacture of knife blades found it to be
‘harder’, ‘rawer’, and ‘less manageable’ than English shear steel. Only
Cockshutt at Wortley employed imported German steel on account of its
hardness for the manufacture of drawing-plates used for drawing steel wire.'

Lewis wrote:

 'Double Spur (steel) - the hardest of all double spur and star; this is
used
 chiefly for gravers; razors also are made of it and fine scissors. These
steels are made chiefly near Newcastle; Mr Cockshutt makes them of late, but
his are not in such repute; uncertain whether from their being  really
inferior, or from their character not being yet established.'

    To my mind Lewis is describing a method, adopted by Cockshutt,  of using
Swedish iron and not English iron for the steel from which he made wire
draw-plates. Cockshutt’s connections with the Fell ‘Steele Trade’ surely
would have provided him with a ready supply of the type of steel that he had
found most suitable for his purposes?
    There is also the possibility that the excavated structure was the
foundation of a steam boiler, erected by a later operator of the Iron Works,
Vincent Corbett, to drive his steam hammer lifting gear that he experimented
with in 1840. It was reported that this contrivance was hidden behind a high
brick wall, but was destroyed by Corbett’s workmen who did not like the
‘new-fangled’ invention.
    Lewis also described the method Cockshutt adopted for the manufacture of
wire-drawing plates.  Cockshutt took a plate of wrought iron and formed it
into a sort of cricket bat shape but flat on both sides. He folded it over,
at the ‘bat’ end to form a narrow ‘U’ section and scratched or filed
grooves across the two inner faces. He then filled the cavity with ‘melted
wild steel’.    He used ‘wild German steel’, from Tyrol or Styria. The
filled end was then heated and forged so forming a composite section of
iron,
steel,  iron, the grooves previously cut across the inner faces served to
grip the steel interior. The holes through which the wire was drawn were
then
punched through, three holes being placed across the width in several rows
along its length. To reclaim old worn-out plates they were heated and the
steel centre was removed by knocking it out. Lewis wrote that this German
wild steel could be filed after forging it and that it would bear holes to
be
‘knocked through’.

Just another question regarding the history of the Wortley Iron Works that
may never be satisfactorily answered.

Regards,

Chris Morley

Top of Message | Previous Page | Permalink

JiscMail Tools


RSS Feeds and Sharing


Advanced Options


Archives

April 2024
March 2024
February 2024
January 2024
December 2023
November 2023
October 2023
September 2023
August 2023
July 2023
June 2023
May 2023
April 2023
March 2023
February 2023
January 2023
December 2022
November 2022
October 2022
September 2022
August 2022
July 2022
June 2022
May 2022
April 2022
March 2022
February 2022
January 2022
December 2021
November 2021
October 2021
September 2021
August 2021
July 2021
June 2021
May 2021
April 2021
March 2021
February 2021
January 2021
December 2020
November 2020
October 2020
September 2020
August 2020
July 2020
June 2020
May 2020
April 2020
March 2020
February 2020
January 2020
December 2019
November 2019
October 2019
September 2019
August 2019
July 2019
June 2019
May 2019
April 2019
March 2019
February 2019
January 2019
December 2018
November 2018
October 2018
September 2018
August 2018
July 2018
June 2018
May 2018
April 2018
March 2018
February 2018
January 2018
December 2017
November 2017
October 2017
September 2017
August 2017
July 2017
June 2017
May 2017
April 2017
March 2017
February 2017
January 2017
December 2016
November 2016
October 2016
September 2016
August 2016
July 2016
June 2016
May 2016
April 2016
March 2016
February 2016
January 2016
December 2015
November 2015
October 2015
September 2015
August 2015
July 2015
June 2015
May 2015
April 2015
March 2015
February 2015
January 2015
December 2014
November 2014
October 2014
September 2014
August 2014
July 2014
June 2014
May 2014
April 2014
March 2014
February 2014
January 2014
December 2013
November 2013
October 2013
September 2013
August 2013
July 2013
June 2013
May 2013
April 2013
March 2013
February 2013
January 2013
December 2012
November 2012
October 2012
September 2012
August 2012
July 2012
June 2012
May 2012
April 2012
March 2012
February 2012
January 2012
December 2011
November 2011
October 2011
September 2011
August 2011
July 2011
June 2011
May 2011
April 2011
March 2011
February 2011
January 2011
December 2010
November 2010
October 2010
September 2010
August 2010
July 2010
June 2010
May 2010
April 2010
March 2010
February 2010
January 2010
December 2009
November 2009
October 2009
September 2009
August 2009
July 2009
June 2009
May 2009
April 2009
March 2009
February 2009
January 2009
December 2008
November 2008
October 2008
September 2008
August 2008
July 2008
June 2008
May 2008
April 2008
March 2008
February 2008
January 2008
December 2007
November 2007
October 2007
September 2007
August 2007
July 2007
June 2007
May 2007
April 2007
March 2007
February 2007
January 2007
2006
2005
2004
2003
2002
2001
2000
1999
1998


JiscMail is a Jisc service.

View our service policies at https://www.jiscmail.ac.uk/policyandsecurity/ and Jisc's privacy policy at https://www.jisc.ac.uk/website/privacy-notice

For help and support help@jisc.ac.uk

Secured by F-Secure Anti-Virus CataList Email List Search Powered by the LISTSERV Email List Manager