Dear Dr. Scott,
Have you consulted the "Pirotechnia" by Biringuccio on this topic? I have
to believe that any of the sources of silver in Italy mentioned by him had
been known since ancient times. The Greek colonial cities in the Italian
part of Magna Graecia coined silver three centuries before the Romans did.
The silver surely wasn't all imported.
Regards,
Jack Lifton
|