another useful aid might be "Metallography and microstructure of ancient and historic metals" David A. Scott 1991 Getty Museum/ Archetype Press: Los Angeles....I know that there are about 250 copies still available from Getty Trust Publications priced about $40.00....this is an introductory text to the subject and includes many etching recipes...David
%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
|