Justine Bayley wrote: > Anders > > Copper alloy coatings on iron objects are not uncommon finds in Britain. .... How these coatings have been achieved ? Ingo Keesmann %%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%