Dear all,
I have just updated my web-site with a couple of articles which may
be of interest:
http://staff.hum.ku.dk/dbwagner/Enc.It/Enc.It.html , an article in
English on the iron industry of the Han period in China, both
technical and historical. This is in a way an abridged version of my
forthcoming book, _The state and the iron industry in Han China_.
http://staff.hum.ku.dk/dbwagner/kons/kons.html , two lectures given
in 1987 in Danish for museum conservators on the metallurgy and
history of cast iron. The bibliography includes a good deal in
English (and some in German and French) which may be of interest to
archaeometallurgists.
In addition, please note that my publication list, at
http://staff.hum.ku.dk/dbwagner/ , includes a number of other studies
of archaeometallurgical subjects, most but not all relating to China.
About half of these are directly available as Web versions. Not all
are included in Chris's archaeometallurgical bibliography at
http://users.ox.ac.uk/~salter/met-bib.htm .
Regards,
Don Wagner
--
--------------------------------------------------------------------------------
lektor dr.phil. Donald B. Wagner
Asien-instituttet / Department of Asian Studies, University of Copenhagen
Leifsgade 33, DK-2300 Copenhagen S, Denmark
tel. +45-3532 8825 fax. +45-3532 8835
http://staff.hum.ku.dk/dbwagner
Note change of e-mail address: <[log in to unmask]>
--------------------------------------------------------------------------------
%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
|