Richard,
I would hope that I am not the only one that would also be interested in
the questions you have about the re-casting of the Nahal Mishmar metal
objects.
would you mind posing your questions to the group?
Aaron Shugar
Institute of Archaeology
University College London
London, WC1H 0PY
At 11:13 AM 4/18/00 -0400, you wrote:
>Hello all,
>I have just read Sariel Shalev's article on recasting the Nahal Mishmar
hoard finds
>and have a few questions. Is Sariel on the list or could someone aid me in
more
>personal communications?
>
>Richard Furrer
>
>
>
%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
|