Jay Woods wrote
>Neither limestone nor dolomite melt at 1 bar. They give off CO2 and form a
powder<
Not necessarily a powder. We used to screeen out the powder and just use the
lumps (from gas fired kilns). There is less sulphur in the lime that way.
Peter Hutchison
%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
|