The lead oxides must surely over the years have been at least partially
conveted to basic lead carbonate which could have converted the powdery
deposit one would expect to a cement-like coating such as occurs (thinly) on
occasion on buried lead pipe. It ocurs even more thinly on all exposed lead.
Peter
Peter Hutchison
[log in to unmask]
%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
|