Marcel J. Thieblot has done a nice study of many varieties of
charcoal-making techniques in Brazil, but stops short of briquetting
technology. This is in Escuros artesaos de uma valiosa energia:
Carvoeiros e carvao de lenha, published in 1984 by the Escola de
Folclore, Sao Paulo.
-Ron Reno
%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
|