The giant bronze statue of Buddha in the Todaiji temple at Nara (Japan)
has been estimated to weigh 450 tons.
It was probably cast in a series of sections over several years, but the
join-lines are almost imperceptible.
I can imagine that something smaller and inverted could be used as a
watertight storage receptable.
Alan Williams
%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%
|