In China, cast iron moulds for casting cast iron have been founded in several archaeology sites, such as Xinglong County of Hebei Province the date was about the late of Warring States Period (5~2c. B.C.); Xin'an County of Henan Province the date was the Han Dynasty (2c.B.C. ~cc.A.D.), and so on.
Chen Jianli
----------------------------------------------
Institute of Historical Metallurgy & Materials
University of Science & Technology,Beijing
No. 30, Xueyuan Road
Beijing, 100083
P. R. China
email: [log in to unmask]
Tel: +86-10-62332534, 62334901
Fax: +86-10-62334901
|